MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Zytel® RS 30G30L NC010 Nylon 610 (Extended Tabular Stress-Strain Data)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion

Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer

Former DuPont product acquired by Celanese in 2022.

Key Words: PA610-GF30
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/cc
 1.31 g/ccDAM; ISO 1183
Moisture Absorption 1.20 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity 93100 cP
@Shear Rate 5000 1/s,
Temperature 280 °C
ISO 11403-1 -2
 123000 cP
@Shear Rate 5000 1/s,
Temperature 260 °C
ISO 11403-1 -2
 135400 cP
@Shear Rate 5000 1/s,
Temperature 250 °C
ISO 11403-1 -2
 305600 cP
@Shear Rate 500 1/s,
Temperature 280 °C
ISO 11403-1 -2
 420900 cP
@Shear Rate 500 1/s,
Temperature 260 °C
ISO 11403-1 -2
 491800 cP
@Shear Rate 500 1/s,
Temperature 250 °C
ISO 11403-1 -2
Linear Mold Shrinkage, Flow 0.0020 cm/cmDAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmDAM; ISO 294-4 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPa50%RH; ISO 527-1/-2
 160 MPaDAM; ISO 527-1/-2
Tensile Stress at Strain 7.36 MPa
@Strain 0.23 %,
Temperature 150 °C
50%RH; ISO 11403-1 -2
 8.44 MPa
@Strain 0.18 %,
Temperature 90.0 °C
50%RH; ISO 11403-1 -2
 10.17 MPa
@Strain 0.31 %,
Temperature 150 °C
DAM; ISO 11403-1 -2
 10.94 MPa
@Strain 0.19 %,
Temperature 40.0 °C
50%RH; ISO 11403-1 -2
 16.49 MPa
@Strain 0.22 %,
Temperature 23.0 °C
50%RH; ISO 11403-1 -2
 18.68 MPa
@Strain 0.21 %,
Temperature 0.000 °C
50%RH; ISO 11403-1 -2
 19.66 MPa
@Strain 0.24 %,
Temperature 40.0 °C
DAM; ISO 11403-1 -2
 19.79 MPa
@Strain 0.46 %,
Temperature 90.0 °C
DAM; ISO 11403-1 -2
 20.88 MPa
@Strain 0.23 %,
Temperature 23.0 °C
DAM; ISO 11403-1 -2
 22.51 MPa
@Strain 0.23 %,
Temperature 0.000 °C
DAM; ISO 11403-1 -2
 25.2 MPa
@Strain 0.25 %,
Temperature -40.0 °C
50%RH; ISO 11403-1 -2
 28.2 MPa
@Strain 1.23 %,
Temperature 150 °C
50%RH; ISO 11403-1 -2
 30.63 MPa
@Strain 0.86 %,
Temperature 90.0 °C
50%RH; ISO 11403-1 -2
 39.8 MPa
@Strain 0.84 %,
Temperature 40.0 °C
50%RH; ISO 11403-1 -2
 40.34 MPa
@Strain 0.37 %,
Temperature -40.0 °C
DAM; ISO 11403-1 -2
 40.58 MPa
@Strain 2.48 %,
Temperature 150 °C
50%RH; ISO 11403-1 -2
 41.59 MPa
@Strain 2.31 %,
Temperature 150 °C
DAM; ISO 11403-1 -2
 48.43 MPa
@Strain 3.85 %,
Temperature 150 °C
50%RH; ISO 11403-1 -2
 49.23 MPa
@Strain 1.78 %,
Temperature 90.0 °C
50%RH; ISO 11403-1 -2
 49.24 MPa
@Strain 0.57 %,
Temperature 0.000 °C
50%RH; ISO 11403-1 -2
 49.35 MPa
@Strain 0.78 %,
Temperature 23.0 °C
50%RH; ISO 11403-1 -2
 53.28 MPa
@Strain 1.82 %,
Temperature 90.0 °C
DAM; ISO 11403-1 -2
 55.92 MPa
@Strain 4.5 %,
Temperature 150 °C
DAM; ISO 11403-1 -2
 62.58 MPa
@Strain 0.73 %,
Temperature 23.0 °C
DAM; ISO 11403-1 -2
 62.93 MPa
@Strain 0.85 %,
Temperature 40.0 °C
DAM; ISO 11403-1 -2
 63.21 MPa
@Strain 2.95 %,
Temperature 90.0 °C
50%RH; ISO 11403-1 -2
 64.45 MPa
@Strain 1.63 %,
Temperature 40.0 °C
50%RH; ISO 11403-1 -2
 64.96 MPa
@Strain 6.96 %,
Temperature 150 °C
DAM; ISO 11403-1 -2
 65.29 MPa
@Strain 0.73 %,
Temperature 0.000 °C
DAM; ISO 11403-1 -2
 72.39 MPa
@Strain 0.77 %,
Temperature -40.0 °C
50%RH; ISO 11403-1 -2
 75.33 MPa
@Strain 3.49 %,
Temperature 90.0 °C
DAM; ISO 11403-1 -2
 79.52 MPa
@Strain 1.49 %,
Temperature 23.0 °C
50%RH; ISO 11403-1 -2
 85.03 MPa
@Strain 2.63 %,
Temperature 40.0 °C
50%RH; ISO 11403-1 -2
 87.13 MPa
@Strain 1.11 %,
Temperature 0.000 °C
50%RH; ISO 11403-1 -2
 88.37 MPa
@Strain 5.52 %,
Temperature 90.0 °C
DAM; ISO 11403-1 -2
 98.25 MPa
@Strain 0.94 %,
Temperature -40.0 °C
DAM; ISO 11403-1 -2
 98.66 MPa
@Strain 1.7 %,
Temperature 40.0 °C
DAM; ISO 11403-1 -2
 102.87 MPa
@Strain 1.34 %,
Temperature 23.0 °C
DAM; ISO 11403-1 -2
 103.81 MPa
@Strain 2.37 %,
Temperature 23.0 °C
50%RH; ISO 11403-1 -2
 109.37 MPa
@Strain 1.34 %,
Temperature 0.000 °C
DAM; ISO 11403-1 -2
 113.84 MPa
@Strain 1.31 %,
Temperature -40.0 °C
50%RH; ISO 11403-1 -2
 121.6 MPa
@Strain 1.79 %,
Temperature 0.000 °C
50%RH; ISO 11403-1 -2
 123.05 MPa
@Strain 2.83 %,
Temperature 40.0 °C
DAM; ISO 11403-1 -2
 135.14 MPa
@Strain 2.05 %,
Temperature 23.0 °C
DAM; ISO 11403-1 -2
 148.56 MPa
@Strain 2.06 %,
Temperature 0.000 °C
DAM; ISO 11403-1 -2
 150.01 MPa
@Strain 1.54 %,
Temperature -40.0 °C
DAM; ISO 11403-1 -2
 151.29 MPa
@Strain 1.91 %,
Temperature -40.0 °C
50%RH; ISO 11403-1 -2
 191.87 MPa
@Strain 2.24 %,
Temperature -40.0 °C
DAM; ISO 11403-1 -2
Elongation at Break 5.0 %DAM; ISO 527-1/-2
 7.0 %50%RH; ISO 527-1/-2
Tensile Modulus 6500 MPa50%RH; ISO 527-1/-2
 8500 MPaDAM; ISO 527-1/-2
Secant Modulus 0.902 GPa
@Strain 10.24 %,
Temperature 100 °C
DAM; ISO 11403-1 -2
 1.09 GPa
@Strain 6.56 %,
Temperature 100 °C
50%RH; ISO 11403-1 -2
 1.28 GPa
@Strain 6.73 %,
Temperature 100 °C
DAM; ISO 11403-1 -2
 1.60 GPa
@Strain 4.16 %,
Temperature 100 °C
50%RH; ISO 11403-1 -2
 1.87 GPa
@Strain 5.55 %,
Temperature 40.0 °C
50%RH; ISO 11403-1 -2
 1.92 GPa
@Strain 3.73 %,
Temperature 100 °C
DAM; ISO 11403-1 -2
 1.9991 GPa
@Strain 6.7 %,
Temperature 40.0 °C
DAM; ISO 11403-1 -2
 2.27 GPa
@Strain 2.34 %,
Temperature 100 °C
50%RH; ISO 11403-1 -2
 2.40 GPa
@Strain 5.16 %,
Temperature 23.0 °C
50%RH; ISO 11403-1 -2
 2.78 GPa
@Strain 3.41 %,
Temperature 40.0 °C
50%RH; ISO 11403-1 -2
 2.94 GPa
@Strain 1.48 %,
Temperature 100 °C
DAM; ISO 11403-1 -2
 3.184 GPa
@Strain 1 %,
Temperature 100 °C
50%RH; ISO 11403-1 -2
 3.45 GPa
@Strain 3.83 %,
Temperature 40.0 °C
DAM; ISO 11403-1 -2
 3.47 GPa
@Strain 4.69 %,
Temperature 23.0 °C
DAM; ISO 11403-1 -2
 3.70 GPa
@Strain 1.95 %,
Temperature 40.0 °C
50%RH; ISO 11403-1 -2
 3.78 GPa
@Strain 3.06 %,
Temperature 23.0 °C
50%RH; ISO 11403-1 -2
 4.15 GPa
@Strain 0.21 %,
Temperature 100 °C
50%RH; ISO 11403-1 -2
 4.18 GPa
@Strain 3.84 %,
Temperature 0.000 °C
50%RH; ISO 11403-1 -2
 4.25 GPa
@Strain 0.21 %,
Temperature 100 °C
DAM; ISO 11403-1 -2
 4.35 GPa
@Strain 4.36 %,
Temperature 0.000 °C
DAM; ISO 11403-1 -2
 4.7381 GPa
@Strain 0.84 %,
Temperature 40.0 °C
50%RH; ISO 11403-1 -2
 5.02 GPa
@Strain 1.76 %,
Temperature 23.0 °C
50%RH; ISO 11403-1 -2
 5.30 GPa
@Strain 2.04 %,
Temperature 40.0 °C
DAM; ISO 11403-1 -2
 5.76 GPa
@Strain 0.19 %,
Temperature 40.0 °C
50%RH; ISO 11403-1 -2
 5.78 GPa
@Strain 2.62 %,
Temperature 23.0 °C
DAM; ISO 11403-1 -2
 6.03 GPa
@Strain 2.31 %,
Temperature 0.000 °C
50%RH; ISO 11403-1 -2
 6.33 GPa
@Strain 0.78 %,
Temperature 23.0 °C
50%RH; ISO 11403-1 -2
 6.52 GPa
@Strain 2.59 %,
Temperature 0.000 °C
DAM; ISO 11403-1 -2
 7.30 GPa
@Strain 1.57 %,
Temperature 23.0 °C
DAM; ISO 11403-1 -2
 7.37 GPa
@Strain 2.37 %,
Temperature -40.0 °C
50%RH; ISO 11403-1 -2
 7.40 GPa
@Strain 0.85 %,
Temperature 40.0 °C
DAM; ISO 11403-1 -2
 7.49 GPa
@Strain 1.33 %,
Temperature 0.000 °C
50%RH; ISO 11403-1 -2
 7.50 GPa
@Strain 0.22 %,
Temperature 23.0 °C
50%RH; ISO 11403-1 -2
 7.82 GPa
@Strain 2.73 %,
Temperature -40.0 °C
DAM; ISO 11403-1 -2
 7.89 GPa
@Strain 1.56 %,
Temperature 0.000 °C
DAM; ISO 11403-1 -2
 8.19 GPa
@Strain 0.24 %,
Temperature 40.0 °C
DAM; ISO 11403-1 -2
 8.44 GPa
@Strain 1.5 %,
Temperature -40.0 °C
50%RH; ISO 11403-1 -2
 8.5726 GPa
@Strain 0.73 %,
Temperature 23.0 °C
DAM; ISO 11403-1 -2
 8.6386 GPa
@Strain 0.57 %,
Temperature 0.000 °C
50%RH; ISO 11403-1 -2
 8.90 GPa
@Strain 0.21 %,
Temperature 0.000 °C
50%RH; ISO 11403-1 -2
 8.94 GPa
@Strain 0.73 %,
Temperature 0.000 °C
DAM; ISO 11403-1 -2
 9.08 GPa
@Strain 0.23 %,
Temperature 23.0 °C
DAM; ISO 11403-1 -2
 9.37 GPa
@Strain 1.76 %,
Temperature -40.0 °C
DAM; ISO 11403-1 -2
 9.4013 GPa
@Strain 0.77 %,
Temperature -40.0 °C
50%RH; ISO 11403-1 -2
 9.79 GPa
@Strain 0.23 %,
Temperature 0.000 °C
DAM; ISO 11403-1 -2
 10.08 GPa
@Strain 0.25 %,
Temperature -40.0 °C
50%RH; ISO 11403-1 -2
 10.5 GPa
@Strain 0.94 %,
Temperature -40.0 °C
DAM; ISO 11403-1 -2
 10.9 GPa
@Strain 0.37 %,
Temperature -40.0 °C
DAM; ISO 11403-1 -2
Izod Impact, Notched (ISO) 16.0 kJ/m²DAM; ISO 180/1A
 17.0 kJ/m²50%RH; ISO 180/1A
Charpy Impact Unnotched 95.0 kJ/m²DAM; ISO 179/1eU
 95.0 kJ/m²50%RH; ISO 179/1eU
Charpy Impact, Notched 16.5 kJ/m²DAM; ISO 179/1eA
 16.5 kJ/m²50%RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 2.28 J/g-°C
Thermal Conductivity 0.260 W/m-Kof melt
Melting Point 224 °CDAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 200 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 50.0 °CDAM; 10°C/min; ISO 11357-1/-2
 
Descriptive Properties
AdditivesLubricants
 Release agent
Delivery formPellets
Part Marking Code>PA610-GF30<ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA610-GF30ISO 1043
Special characteristicsLight stabilized or stable to light

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZDSY5475a / 238181

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.