MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: This is a Non-Halogenated Flame Retardant Grade. Used in electronic and telecommunications enclosures, computer equipment, appliances.

Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Linear Mold Shrinkage 0.004 - 0.006 cm/cmASTM D955
Melt Flow 12 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 13 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 8700 psi
@Thickness 3.17 mm
ASTM D638
Elongation at Break 65 %
@Thickness 3.17 mm
ASTM D638
Flexural Yield Strength 12900 psi
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 390000 psi
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 11.0 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index >= 600 VPLC 0
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness 1.50 mm
PLC 3
 15 - 30 sec
@Thickness 2.50 mm
PLC 3
 30 - 60 sec
@Thickness 3.00 mm
PLC 2
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness 1.50 mm
PLC 1
 60 - 120 arcs
@Thickness 2.50 mm
PLC 1
 60 - 120 arcs
@Thickness 3.00 mm
PLC 1
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minPLC 3
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 205 °F
@Thickness 3.17 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CASTM D648
 185 °F
@Thickness 3.17 mm
ASTM D648
Vicat Softening Point 230 °C
UL RTI, Electrical 60.0 °C
UL RTI, Mechanical with Impact 60.0 °C
UL RTI, Mechanical without Impact 60.0 °C
Flammability, UL94 V-0
@Thickness 1.50 mm
all colors; UL file E155285
 5VB
@Thickness 2.00 mm
all colors; UL file E155285
 5VA
@Thickness 2.50 mm
 5VA
@Thickness 3.0 mm
all colors; UL file E155285
Glow Wire Ignition Temperature 700 °C
@Thickness 2.00 mm
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 925 °C
@Thickness 1.50 mm
IEC 60695-2-12
 925 °C
@Thickness 2.00 mm
IEC 60695-2-12
 950 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 232 - 266 °C
Middle Barrel Temperature 246 - 274 °C
Front Barrel Temperature 246 - 288 °C
Melt Temperature 246 - 288 °C
Mold Temperature 57.2 - 85.0 °Csurface
Drying Temperature 87.0 °C
@Time 10800 - 14400 sec
Injection Pressure 10000 - 16000 psi
Back Pressure 25.0 - 100 psi
Screw Speed 25 - 75 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose
PTS PCA-2201NH-V Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
BASF Ultramid® 8202 PA6 (Dry)
Celanese Celstran® TPU-GF30-01-US TPU, 30% Glass Reinforced

PZ9PU42r / 143021

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.