MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATG s.r.l. XNBR Carboxylated Nitrile Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50 - 95
Tensile Strength, Ultimate 8.00 - 23.0 MPa
Elongation at Break 200 - 725 %
Rebound 10 - 45 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Minimum Service Temperature, Air -45.0 °C
 
Descriptive Properties
Abrasion Resistancehigh
Chemical Resistance to Animal and Vegetable Oils and Greaseshigh
Chemical Resistance to Aromatic Hydrocarbonslow
Chemical Resistance to Chloride Solventsnone
Chemical Resistance to Distilled Waterhigh
Chemical Resistance to Ketonesnone
Chemical Resistance to Maximum Concentrated Alkalis (at 50°C)medium
Chemical Resistance to Medium-High Concentrated Acids (at 50°C)none
Chemical Resistance to Mineral Oils and Aliphatic Hydrocarbonsmedium
Compression set at 100°Cmedium
Impermeability at gas (Oxygen and Nitrogen)medium
Resistance to Flamenone
Resistance to Heat Agingmedium
Resistance to Low Temperaturesmedium
Resistance to Ozone and Weatheringmedium
Tear Strengthmedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATG s.r.l. NBR Nitrile-Butadiene Rubber
Hydrogenated Nitrile Rubber (HNBR)
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
ATG s.r.l. AU-EU Polyurethane Rubber
Monmouth Rubber & Plastics Durafoam™ C41NBR Nitrile Rubber

PATG010 / 79375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.