MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Nucrel® 30707HS Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Acrylic Acid

Material Notes: 7 wt% Acrylic Acid.

Nucrel® 30707HS is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins.

Features/Benefits: Low seal initiation temperature allows high-speed packaging. Very good hot tack, seal through contamination, and heat seal strength provides strong, reliable heat seals. Balanced acid content (7% AA) provides good adhesion to both aluminum foil and low-density polyethylene (LDPE). In extrusion coating applications, 7 MFI provides better performance in internally deckled dies compared to higher MFI extrusion coating resins. Higher drawability for thinner coatings and/or higher extrusion speeds.

Typical Applications: Cable shield wrap. Sealants for sachets in both food and nonfood applications. Toothpaste tubes, as a foil/LDPE tie layer. Other foil-containing pouches and sachets. Medical/pharmaceutical packaging.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Seal Strength 1800 g/25 mmseal bar 150°C.
Hot Tack Strength 1250 g/25 mmseal bar 110°C; Packforsk method.
 
Thermal PropertiesOriginal ValueComments
Melting Point 84.0 °CFreezing Point via DSC/ASTM D3418
 102 °CUpon Melting via DSC/ASTM D3418
Vicat Softening Point 86.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 °CTypical Die Temp. for Extrusion Coating
Melt Temperature 220 - 305 °CExtrusion Coating

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin
Arkema LOTRYL® 37 EH 550 Copolymer Ethylene - Acrylic Ester
Honeywell A-C® 540A EAA copolymer
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
Dow Primacor® 3460 Ethylene Acrylic Acid (EAA)

PDUPJJ / 33653

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.