MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Northstar Polymers MSS-A90A High Performance Polyurethane Cast Elastomer System 90A
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasion resistance, slow response speed, and low energy rebound/response. Ester base systems are generally less expensive than PTMEG base material. Possible applications for this material include skirting for conveyer belts, abrasion resistance liners and parts, and other specialty parts. This is a conventional “full-prepolymer” type material cured with 1,4 BDO. Can be approved for FDA dry food contact.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D2240
Tensile Strength 4200 psiASTM D412
Elongation at Break 650 %ASTM D412
Rebound 28 %Bashore Rebound; ASTM D2632
Tear Strength 300 pliSplit; ASTM D624
 600 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 62ASTM D4060
 
Processing PropertiesOriginal ValueComments
Processing Temperature 77.0 °FCuring Agent Temperature
 180 - 200 °FPrepolymer Temperature
Mold Temperature 180 - 200 °F
Cure Time 0.500 hour
@Temperature 93.3 °C
De-mold Time
 16.0 hour
@Temperature 82.2 °C
Complete Cure Cycle
Pot Life 2.50 - 3.00 min
 
Descriptive Properties
Curing AgentBNA-005
PrepolymerMSA-052

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mearthane Durethane™ S DS-290A Solid Polyurethane Elastomer
Mearthane Durethane™ M DM-640A Foam Polyurethane
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade
Dow SE SLR-4610 Solution polymerized Styrene Butadiene Rubber (S-SBR)

PNORTH07 / 54842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.