MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quantum Composites QC-2130 Phenolic 25% Glass Fiber SMC  (discontinued **)
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Phenolic; Phenolic/Glass Fiber SMC

Material Notes: QC-2130 is a glass-reinforced sheet molding compound based on a phenolic resin matrix. It exhibits outstanding low flammability characteristics. QC-2130 is recommended for applications such as aircraft interiors and public transportation components requiring composite materials having very low flammability, low smoke, and minimal generation of toxic gases. Form and Color = Roll, Natural & Black. Glass Length = 1 inch.

A. Schulman has acquired Quantum Composites.

Key Words: Sheet Molding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 75.0 MPaASTM D638
Tensile Modulus 13.0 GPaASTM D638
Flexural Yield Strength 137 MPaASTM D790
Flexural Modulus 9.00 GPaASTM D790
Izod Impact, Notched 2.67 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 1.00 mm
5V
Oxygen Index 46 %ASTM D2863
Shrinkage 0.0010 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 132 - 160 °CMold temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fiberglass Search Hints
PTS Trilac® ABS-GF3000-BK 30% Fiberglass Black ABS Resin
G-3 Fiberglass Phenolic Laminate Sheet
Quantum Composites Lytex® 9063 63% Glass Fiber Epoxy SMC
Röchling GLASTHERM HT Insulation Sheet

PCOQC2 / 29039

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.