3M VFP-876 is the most flexible of the heat-shrinkable, polyolefin tubings. Rated at 135°C. VFP-876 Tubing has been engineered to offer a low shrink temperature of 100°C. This allows the tubing to shrink rapidly, thereby minimizing heat exposure and possible damage to sensitive substrate materials or components. VFP-876 Tubing meets MIL-R-46846, Type V and AMS-3587 and is UL Recognized (UL File Nos. E-39100 and E-69751). It is rated for continuous operation from -55°C to 135°C and withstands elevated temperatures to 300°C for brief periods.Information provided by 3M |