MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lucite International XL Sanitary Ware Acrylic Sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.

Benefits: Smooth surface; Infinite colors and effects; Hardwearing; Exceptional quality; 100% recyclable; Enhanced functionality

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Water Absorption 0.25 %ASTM D570
Linear Mold Shrinkage <= 0.025 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 95ASTM D785 Procedure A
Tensile Strength 62.0 - 69.0 MPaspecimen type 1, 5 mm/mn; ASTM D638
Elongation at Break 4.0 - 5.0 %
Modulus of Elasticity 3.172 GPa
Flexural Strength 110.3 MPaASTM D790 (Method 1, Procedure A)
Compressive Yield Strength 111 MPaASTM D695
Shear Strength 59.6 MPa
Izod Impact, Notched 16.0 J/mASTM D256 method C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance <= 1.00e+14 ohm
@Temperature 28.0 °C
75% RH; ASTM D257
Dielectric Constant 3.0
@Frequency 1000 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
 4.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mmshort time test; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°CASTM D696
Specific Heat Capacity 1.47 J/g-°CASTM C351
Thermal Conductivity 0.209 W/m-KASTM C177-76
Maximum Service Temperature, Air 80.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °CASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 190 °Cthermoforming temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Cast
Röhm Acrylite® 249 Acrylic Sheet, Aerospace Grade
Polycasa CAST PMMA
Clax Italia Perclax® Cast Acrylic
Clax Italia AQuariA® Cast Acrylic

PLUCIT9403 / 150117

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.