MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kazanorgsintez Alpha-Methylstyrene Fraction
Categories: Fluid

Material Notes: Production Method: Alpha-methylstyrene fraction is a by-product of the production of phenol and acetone by the cumene method.

Application: Used for the production of marketable alpha-methylstyrene

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 0.900 g/cc2nd Grade
 0.907 - 0.910 g/cc
@Temperature 20.0 °C
1st Grade
 
Optical PropertiesOriginal ValueComments
Refractive Index >= 1.5322nd Grade
 1.536 - 1.53881st Grade
 
Descriptive Properties
Mass Content (%)0.002Mass content of phenol, 1st and 2nd Grade
 0.5Mass content of N-propylbenzene and styrene, 1st Grade
 0.5Mass content of butyl benzene, 1st Grade
 0.7Mass content of butyl benzene, 2nd Grade
 90Mass content of alpha-methyl styrene, 2nd Grade
 95Mass content of alpha-methyl styrene, 1st Grade

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKAZAN180 / 127499

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.