MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Dow™ 5004I LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description: Dow LDPE 5004I is used for fresh milk cartons, liquid/juice containers, dry foods packaging, snack foods packaging, moist foods packaging, and medical packaging. Dow LDPE extrusion coating resins provide optimal neck-in and draw-down performance with minimal taste/odor contribution.
  • A low melt index coating resin for demanding packaging applications

Complies with: US FDA 21 CFR 177.1520©2.2a; US FDA DMF; Canadian HPFB No Objection (With Limitations); EU No 10/2011; Japan Hygienic Olefin and Styrene Plastics Association. Consult the regulations for complete details.

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; FDA 21 CFR 177.1520©2.2; EU No 10/2011; Canadian HPFB No Objection (With Limitations); JHOSPA

Form: Pellets

Processing Method: Cast Film; Extrusion Coating

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D792
Water Vapor Transmission 23.3 g/m²/day1.50 g/100 in²/day1.0 mil, Extrusion Coating; ASTM F1249
Melt Flow 4.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In 6.35 cm
@Temperature 321 °C
2.50 in
@Temperature 610 °F
1.0 mil
Coating Weight 7.04 g/m²4.40 lb/ream
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 14.8 MPa
@Thickness 0.0254 mm
2140 psi
@Thickness 0.00100 in
Cast Film; ASTM D882
Film Tensile Strength at Yield, TD 10.9 MPa
@Thickness 0.0254 mm
1580 psi
@Thickness 0.00100 in
Cast Film; ASTM D882
Film Elongation at Break, MD 220 %
@Thickness 0.0254 mm
220 %
@Thickness 0.00100 in
Cast Film; ASTM D882
Film Elongation at Break, TD 610 %
@Thickness 0.0254 mm
610 %
@Thickness 0.00100 in
Cast Film; ASTM D882
Coefficient of Friction, Dynamic 0.450.45vs. Itself; ASTM D1894
Elmendorf Tear Strength MD 310 g
@Thickness 0.0254 mm
310 g
@Thickness 0.00100 in
Cast Film; ASTM D1922
Elmendorf Tear Strength TD 80 g
@Thickness 0.0254 mm
80 g
@Thickness 0.00100 in
Cast Film; ASTM D1922
Dart Drop Test 27.0 g
@Thickness 0.0254 mm
0.0595 lb
@Thickness 0.00100 in
Cast Film; ASTM D1709A
Film Tensile Strength at Break, MD 31.0 MPa
@Thickness 0.0254 mm
4500 psi
@Thickness 0.00100 in
Cast Film; ASTM D882
Film Tensile Strength at Break, TD 17.0 MPa
@Thickness 0.0254 mm
2470 psi
@Thickness 0.00100 in
Cast Film; ASTM D882
Heat Seal Strength Initiation Temperature 105 °C221 °F1.0 mil, Extrusion Coating
 
Thermal PropertiesMetricEnglishComments
Melting Point 112 °C234 °F
Vicat Softening Point 95.0 °C203 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 12.9 %
@Thickness 0.0254 mm
12.9 %
@Thickness 0.00100 in
Cast Film; ASTM D1003
Gloss 51 %
@Thickness 0.0254 mm
51 %
@Thickness 0.00100 in
45°, Cast Film; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 316 - 327 °C600 - 620 °F
 
Descriptive Properties
Film Puncture Resistance28 ft-lb/in31.0 mil, Cast Film
Film Toughness1370 ft-lb/in3MD, Cast Film, ASTM D882
 1750 ft-lb/in3TD, Cast Film, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF465 / 311158

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.