MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite NEONIT® SK80 L8G Epoxy Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: NEONIT® SK80 L8G is a long glass fiber reinforced epoxy molding compound with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over molding and manufacturing of large commutators.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 g/ccISO 1183
Apparent Bulk Density 0.650 g/ccISO 60
Water Absorption 0.050 %ISO 62
Linear Mold Shrinkage 0.0011 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 107 MPaISO 527-1
Elongation at Break 0.70 %ISO 527-1
Tensile Modulus 19.0 GPaISO 527-1
Flexural Strength 202 MPaISO 178
Flexural Modulus 15.0 GPaISO 178
Compressive Strength 244 MPaISO 179-1
Charpy Impact, Notched 43.0 kJ/m²ISO 179-1
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 32.0 kV/mmIEC 60243-1
Comparative Tracking Index 200 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 11.0 µm/m-°CTMA
CTE, linear, Transverse to Flow 49.0 µm/m-°CTMA
Glass Transition Temp, Tg 195 °CTMA
Shrinkage -0.0300 %Post; ISO 2577
 
Descriptive Properties
ColorDark Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite NEONIT® SK60 L8F Epoxy Molding Compound
Cosmic Plastics CP7311 Epoxy Molding Compound
Cookson Group Plaskon® 2929BNSC Epoxy Molding Compound
Bakelite® EP 8413 Epoxy Molding Compound
Sumitomo Bakelite NEONIT® K82 L8 Epoxy Molding Compound

PSUMIT177 / 193982

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.