MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Parker Chomerics Tecknit® 0236 Conductive Silicone Sealant/Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Comments: Thick flexible paste

Typical Applications: Bonding Ag/Al elastomer

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.90 g/cc
Volatile Organic Compounds (VOC) Content 259 g/l
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 0.689 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.010 ohm-cm
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Temperature 24.0 °C
Shelf Life 9.00 Month
 
Descriptive Properties
FillerAg/Al
Mix Ratio100:2.04
Resin SystemSilicone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil R-2180 Silicone Engineering Coating
NuSil CF1-6755 Silicone Two Part Sealing & Adhesive
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant
Master Bond MasterSil 152 Silicone

PCHOME417 / 131127

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.