MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem LDF0025 Low density polyethylene of high molecular weight
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: LDF0025 is a low density polyethylene of high molecular weight that provides high mechanical strength. The product is highly versatile and can be used in several applications due to their easy processability and high compatibility with other types of polyethylene. It does not contain antiblock and slip additives.
Applications: Shrink film., bags and sacks, blown film, agricultural films and greenhouse coverings, industrial bags, blends with HDPE and LLDPE for extrusion and molding process, bottles for consumer goods.
Processes: Blown film extrusion. Injection molding.

Film properties tested with a monolayer 50 µm thickness blown film, blow up ratio: 2.8, die gap: 1.8 mm.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccASTM D792
Melt Flow 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 260 %ASTM D882
Film Elongation at Break, TD 550 %ASTM D882
Elmendorf Tear Strength TD 180 gASTM D1922
Dart Drop Test 200 gASTM D1709/A
Film Tensile Strength at Break, MD 30.0 MPaASTM D882
Film Tensile Strength at Break, TD 22.0 MPaASTM D882
1% Secant Modulus, MD 200 MPaASTM D882
1% Secant Modulus, TD 230 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 13 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBRAS623 / 314016

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.