Introduction: Two component filled epoxy system. Solid, very good mechanical and thermic property. Abrasion resistant. Application: Foundry patterns, core box, copy moulds. Cured: 24 h at R.T. (23±2° C) + 15 h at 60° C Information provided by Poolkemie |