Stellite™ 720 UltraFlex™ provides a metallurgically-bonded cladding with minimal dilution to a metal substrate, providing superior wear resistance and exceptionally high corrosion resistance in reducing atmospheres. This cladding may be applied to internal diameters, complex shapes, and non-line-of-sight geometries. This UltraFlex Cladding has been applied with good results on bulk material conveyance pipe, conveyance screws, refinery bends, pump casings, and valve components. Data provided by the Kennametal Conforma Clad Inc. |