MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 7945MP Hi-Performance Acrylic 200MP
Categories: Polymer; Adhesive

Material Notes: This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materials. It features exceptional shear strength and adhesion to high surface energy (HSE) plastics and metal surfaces.

Designed to meet the performance requirements of most membrane keyboards. Outstanding resistance to temperature extremes, chemicals and humidity. Also resists oozing, lifting and separation of switch layers. All products feature 2 mils of 200MP on each side

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 microns1.00 milPolyester
 50.8 microns2.00 milAdhesive
 50.8 microns2.00 milAdhesive
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 0.469 MPa68.0 psiCohesion Dynamic, PET/Stainless Steel; ASTM D1002
 0.483 MPa70.0 psiCohesion Dynamic, PET/Polycarbonate; ASTM D1002
Peel Strength 0.4602 kN/m2.625 pli90° Peel, PET/Aluminum, Initial (20 mins); ASTM D3330
 0.53686 kN/m3.0625 pli90° Peel, PET/PET, Initial (20 mins); ASTM D3330
 0.5478 kN/m3.125 pli90° Peel, PET/Polycarbonate, Initial (20 mins); ASTM D3330
 0.701 kN/m4.00 pli90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330
 0.73407 kN/m4.1875 pli90° Peel, PET/PET, 72 hrs at RT; ASTM D3330
 0.789 kN/m4.50 pli90° Peel, PET/Polycarbonate, 72 hrs at RT; ASTM D3330
 0.920 kN/m5.25 pli90° Peel, PET/Aluminum, 72 hrs at RT; ASTM D3330
 0.920 kN/m5.25 pli90° Peel, PET/Polycarbonate, 72 hrs at 70°C; ASTM D3330
 1.23 kN/m7.00 pli90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330
 1.380 kN/m7.875 pli90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330
 1.797 kN/m10.25 pli90° Peel, PET/Stainless Steel, 72 hrs at 70°C; ASTM D3330
 1.84 kN/m10.5 pli90° Peel, PET/Aluminum, 72 hrs at 70°C0; ASTM D3330
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.70e+14 ohm-cm5.70e+14 ohm-cmASTM D257
Surface Resistance >= 5.60e+16 ohm>= 5.60e+16 ohmASTM D257
Insulation Resistance 1.00e+13 ohm1.00e+13 ohm100VDC, 60 sec; Mil-I-46058C
Dielectric Constant 3.483.48ASTM D150
Dielectric Strength 59.1 kV/mm1500 kV/inASTM D149
Dissipation Factor 0.0160.016ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.10 µm/m-°C
@Temperature 27.0 - 175 °C
3.39 µin/in-°F
@Temperature 80.6 - 347 °F
ASTM D696
 
Descriptive Properties
Adhesive Type200MP
Liner58# PCK 4.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow XU 66129.00 Monolayer Adhesive Film
3M Scotch-Seal™ 2084 Metal Sealant

PMM33308 / 168055

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.