MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexWeb® CFC™-20-1/8-6.0 Composite Flooring Honeycomb Core  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Aramid

Material Notes: Hexweb® CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal configuration, the block is dipped in phenolic resin. After curing the resin, slices are cut to the desired thickness.

Features: Specifically designed for aircraft flooring applications; Superior properties and performance over balsa and foam core materials; Proven durability in extensive flooring tests; Significant weight advantage over balsa and foam core materials; Exceeds all FAA safety requirements; Excellent property retention at 350°F; Moisture and fungus resistant.
Applications: Hexweb® CFC™-20 honeycomb core was specifically developed to provide a tough, lightweight core material for use in aircraft flooring systems. A range of product densities are available to fit a wide variety of loading requirements. The core material when bonded to metallic or nonmetallic facings provides a flooring panel sheet which may be cut or contoured to fit any aircraft flooring module.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.00 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Compressive Yield Strength >= 0.725 ksiBare, min, preliminary value obtained from limited testing
 >= 0.780 ksiStabilized, min, preliminary value obtained from limited testing
 0.965 ksiBare, typical, preliminary value obtained from limited testing
 1.04 ksiStabilized, typical, preliminary value obtained from limited testing
Shear Modulus 8.00 ksiPlate Shear, W Direction, typical, obtained from limited testing
 13.5 ksiPlate Shear, L Direction, typical, obtained from limited testing
Shear Strength >= 0.180 ksiPlate Shear, W Direction, min, preliminary value obtained from limited testing
 0.240 ksiPlate Shear, W Direction, typical, obtained from limited testing
 >= 0.290 ksiPlate Shear, L Direction, min, preliminary value obtained from limited testing
 0.390 ksiPlate Shear, L Direction, typical, obtained from limited testing

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core
Hexcel® HexWeb® HRH-10 - 1/8- 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Ultracor® UCF-51-3/8-2.0 Honeycomb Core Material
Ultracor® UKF-85-1/4-1.5 Honeycomb Core Material

PHEXC317 / 98788

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.