MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Henkel Loctite® Stycast® 2651 with CAT 11 Dielectric Grade Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast 2651 provides the following product characteristics:
  • General purpose
  • Can be used with a variety of catalysts

Application: Encapsulation

Loctite Stycast 2651 is a dielectric grade epoxy encapsulant designed for general purpose applications and has excellent adhesion to a wide variety of substrates.

CATALYST DESCRIPTION

Loctite CAT 11 provides the following product characteristics:

  • Long pot life
  • Excellent chemical resistance
  • Good physical and chemical properties at elevated temperatures

Cure: Heat cure

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³Mixed; ASTM D792
 1.65 g/cc0.0596 lb/in³Part A, Loctite Stycast 2651
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
Boil, Cured
Viscosity 45 cP
@Temperature 65.0 °C
45 cP
@Temperature 149 °F
Part B, Loctite CAT 11
Brookfield Viscosity 25000 cP25000 cPMixed
 225000 cP225000 cPPart A, Loctite Stycast 2651; Spindle 7, speed 5 rpm
Outgassing - Total Mass Loss 0.010 %0.010 %Sample cured 3 hours @ 100ºC; ASTM E 595, CVCM
 0.63 %0.63 %Sample cured 3 hours @ 100ºC; ASTM E 595, TML
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888
Tensile Strength 62.0 MPa8990 psi
Flexural Strength 103 MPa14900 psi
Compressive Strength 110 MPa16000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+15 ohm-cm5.00e+15 ohm-cm
Dielectric Constant  3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
 4.6
@Frequency 1000 Hz
4.6
@Frequency 1000 Hz
 4.8
@Frequency 60 Hz
4.8
@Frequency 60 Hz
Dielectric Strength 17.7 kV/mm450 kV/in
Dissipation Factor  0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
 0.020
@Frequency 60 Hz
0.020
@Frequency 60 Hz
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C22.2 µin/in-°FTMA
Thermal Conductivity 0.660 W/m-K4.58 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 155 °C311 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 - 60.0 min
@Temperature 120 °C
0.500 - 1.00 hour
@Temperature 248 °F
Option 3
 120 - 240 min
@Temperature 100 °C
2.00 - 4.00 hour
@Temperature 212 °F
Option 2
 480 - 960 min
@Temperature 80.0 °C
8.00 - 16.0 hour
@Temperature 176 °F
Option 1
Working Life >= 240 min
@Temperature 25.0 °C
>= 240 min
@Temperature 77.0 °F
100 g
Shelf Life 9.00 Month9.00 MonthPart A, Loctite Stycast 2651, from date of manufacture
 
Descriptive Properties
AppearanceBlackPart A, Loctite Stycast 2651
Mix Ratio, by Volume100 : 12.5Material : Catalyst
Mix Ratio, by Weight100 : 8.5Material : Catalyst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK7921 / 255408

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.