MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott B 270® i Ultra White Glass
Categories: Ceramic; Glass; Optical

Material Notes: SCHOTT offers B 270® i crown glass in sheet glass form suitable for a variety of different market demands, especially suitable for biotech applications. B 270® is amde by a specific up-draw process, offers high stability with respect to solarization in combination with high transmission in the visible wavelength range. It has a firepolished surface and high chemical stability. B 270® i is available in a wide range of thicknesses and various stock formats. Customized formats (e. g. rounds) and processing can be offered upon request. B 270® i is available in a thickness range of 0.9 mm – 10.0 mm.

Applications:

  • CD / DVD Pick up Digital Projection
    • High transmittance
    • Cost efficient processing due to wide thickness range
  • Surface acoustic wave type touch panel
    • Low acoustic attenuation
    • High transmittance
  • Monitor glass for coaters
    • High transmittance
    • Cost efficient process monitoring
  • Substrates for bio-chips (flow cells)
    • Low autofluorescence
    • Fire polished surface

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.56 g/cc
Thickness 900 - 1000 microns
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 7.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.40 µm/m-°C
@Temperature 20.0 - 300 °C
Transformation Temperature, Tg 536 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.522
Transmission, Visible 91.7 %D65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corning Gorilla® Glass 5 Display Glass
Corning Gorilla® Glass SR+ Touch Screen Glass
Schott B270™ Sheet Glass
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.0022" Diameter Wire, High Performance EMC Window
Ohara S-BAH10 Optical Glass

CSGT9947 / 183200

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.