MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Telcar® DE 7052 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Availability: Asia Pacific

Uses: Flexible Grips; Handles; Plugs; Shock Absorbing Pads; Toys

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ASTM D792
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70
@Time 10.0 sec
70
@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 5.00 MPa725 psiASTM D412
Tensile Stress at Strain  3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
ASTM D412
 5.00 MPa
@Strain 300 %
725 psi
@Strain 300 %
ASTM D412
Elongation at Break 380 %380 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 140 - 180 °C284 - 356 °FInjection
Middle Barrel Temperature 140 - 180 °C284 - 356 °FInjection
Front Barrel Temperature 140 - 180 °C284 - 356 °FInjection
Zone 1 140 - 180 °C284 - 356 °FExtrusion
Zone 2 140 - 180 °C284 - 356 °FExtrusion
Zone 3 140 - 180 °C284 - 356 °FExtrusion
Zone 4 140 - 180 °C284 - 356 °FExtrusion
Zone 5 140 - 180 °C284 - 356 °FExtrusion
Die Temperature 140 - 180 °C284 - 356 °FExtrusion
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection
Drying Temperature 40.0 - 80.0 °C104 - 176 °F
Injection Pressure 2.07 - 20.7 MPa300 - 3000 psiInjection
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1593 / 238084

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.