MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating
Categories: Ceramic; Nitride

Material Notes: This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN for hard coat; 634-BN(SC) for softer, lubricious coat.

Key Words: Coatings
Vendors: Aremco’s Pyro-Paint refractory coatings offer the ultimate protection of high temperature graphite, metal and refractory structures used in the processing of ceramics, glasses, metals, and plastics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Solids Content 18 %volume
 19.8 %weight
pH 11 - 12Coating pH
Viscosity 500 - 1500 cP
Thickness 25.4 micronsDry Film Thickness
 142 micronsWet Film Thickness
Storage Temperature 40.0 - 90.0 °F
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1560 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 90.0 °FApplication Temperature
Cure Time 2.00 hour
@Temperature 93.3 °C
>2 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month
 
Descriptive Properties
ColorWhite
Coverage ft2/gal288Theoretical Coverage at 1 mil dry film thickness
Thinner634 BN-T
Weight/Gallon9.5 lbs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials PolarTherm® PT110 Boron Nitride (BN) Powder
Momentive Performance Materials HCV Boron Nitride (BN) Powder
Momentive Performance Materials HBN Hot-Pressed Boron Nitride
H.C. Starck Grade A 01 Boron Nitride, BN
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer

CAREM59 / 600

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.