MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Microtherm Group FreeFlow Pourable Opacified Silica Thermal Insulation Beads
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material

Material Notes: Microtherm® granules for high temperature are a pourable microporous insulation with flow characteristics that make them ideal for the filling of closed objects of complex shape. Microtherm® granules for high temperature offer microporous insulation performance for applications where conventional insulation products simply cannot be used.
    Properties
  • Formulation based on opacified silica.
  • Capable of continuous exposure to 1000 °C (1832 °F).
  • Up to 3 or 4 times more thermally efficient at high temperatures than conventional insulations.
  • Suitable for automated feeding of complex shapes
  • Environmentally safe.
  • Free of harmful respirable fibers.
    Applications
  • Small fuel cells and reformers.
  • Void insulation in furnaces, burners and refractory systems.
  • Void insulation for domestic appliances.
  • Any high temperature application where insulation in the form of conventional panel or block cannot be used.

Information provided by Microtherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.360 - 0.400 g/cc
 0.410 - 0.450 g/ccTap
Bead Size 0.300 - 2.50 mm
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.670 J/g-°C
@Temperature 0.000 °C
 0.820 J/g-°C
@Temperature 100 °C
 0.920 J/g-°C
@Temperature 200 °C
 0.960 J/g-°C
@Temperature 300 °C
 1.00 J/g-°C
@Temperature 400 °C
 1.02 J/g-°C
@Temperature 500 °C
 1.04 J/g-°C
@Temperature 600 °C
Thermal Conductivity 0.0340 W/m-K
@Temperature 100 °C
@ 430 kg/m³
 0.0380 W/m-K
@Temperature 200 °C
@ 430 kg/m³
 0.0420 W/m-K
@Temperature 300 °C
@ 430 kg/m³
 0.0480 W/m-K
@Temperature 400 °C
@ 430 kg/m³
 0.0540 W/m-K
@Temperature 500 °C
@ 430 kg/m³
Maximum Service Temperature, Air 1000 °Cfor long term exposure
Shrinkage <= 3.0 %
@Temperature 1000 °C,
Time 86400 sec
full soak

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Insulfrax® Paper
Microtherm Group Aeroguard® SD Filament Reinforced Silica Thermal Insulation Panel, Flexible
Mica (KAl2(AlSi3O10)(OH)2)
DuPont™ Kapton® 500HN Polyimide Film, 125 Micron Thickness

CMICRO06 / 90048

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.