MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice in applications where added stiffness, rigidity and dimensional stability are required.

Data provided by the manufacturer, Cast Nylons Limited.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccASTM D792
Water Absorption 0.50 - 0.60 %24 hrs; ASTM D570
Water Absorption at Saturation 1.1 - 1.2 %ASTM D570
Deformation 0.40 %ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 116 - 120ASTM D785
Hardness, Shore D 84 - 85ASTM D2240
Tensile Strength 9700 - 11500 psiASTM D638
Elongation at Break 2.0 - 5.5 %ASTM D638
Tensile Modulus 550000 - 750000 psiASTM D638
Flexural Strength 17500 - 18500 psiASTM D790
Flexural Modulus 500 - 570 ksiASTM D790
Compressive Strength 17000 - 17500 psiASTM D695
Compressive Modulus 410000 - 455000 psiASTM D695
Izod Impact, Notched 0.600 - 0.900 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µin/in-°FASTM D696
Melting Point 499 - 501 °FASTM D789
Maximum Service Temperature, Air 230 °FContinuous
 330 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 360 - 370 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 245 - 255 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 105 FR  Polypropylene (PP) Glass Fiber 30% - Flame Retardant
Techmer ES Electrafil® J-1/CF/20 Nylon 66, 20% Carbon Fiber Reinforced
Akro-Plastic Akromid® B3 GF 35 1 black (2486) PA6 , Dry, 35% Glass Filled
Ensinger Tecamid® 6/6 Nylon (PA66)
Ensinger Tecamid® GF30 Extruded Nylon 6/6 30% glass-fiber-reinforced (PA66)

PCAST75 / 149809

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.