MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay Thornel® P-25 2K Carbon Fiber, Pitch Precursor
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Continuous filament strand from a pitch precursor.

2000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 3.1 m/g yield, 0 tpm twist, 0.17 mm² fiber area in yarn cross section.

Solvay has acquired the Thornel product line as a part of the Cytec purchase.

Key Words: Carbon Fibre
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³
Specific Surface Area 0.70 m²/g0.70 m²/g
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1400 MPa203000 psi
Elongation at Break 0.90 %0.90 %
Tensile Modulus 160 GPa23200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00130 ohm-cm0.00130 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 22.0 W/m-K153 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)
Solvay Thornel® Graphite Cloth
Solvay Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Toho Tenax Besfight® MC Type I (3000 Filament) Nickel Coated Carbon Fiber

ETHORD / 6085

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.