MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ELM® SoyGrease™ Premium Biodegradable Food Grade Grease, NLGI Grade 1
Categories: Fluid; Lubricant

Material Notes: Description: Elm ELM SoyGrease™ Food Machinery is formulated with optimized USA grown natural seed oils that surpass the lubricity of most conventional oils. It is formulated in accordance with the criteria established by USDA H-1 and U.S. FDA regulation 21 CFR 178.3570, “Lubricants With Incidental Food Contact.” It has been approved by the NSF.

Applications: Meets the demanding applications of the food processing and beverage industries. Excellent for lubrication of bearing, grease lubricated gears, and machine slides

Benefits:

  • Superior lubricity protects moving parts
  • Extreme pressure additives protect under heavy shock loads
  • Protects all ferrous metal components from rust and corrosion
  • Superior adhesion resists water wash out
  • Excellent operating temperature range
  • Meets USDA’s proposed Biobased product definition for EO 13101
  • Meets EPA’s Environmental Preferable Purchasing (EPP) criteria
  • Made from renewable USA-grown crop-based oils
  • Meets State of Iowa Senate File - SF 2185 and 2249

Information provided by ELM®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 213Base Oil, Index
Kinematic Viscosity at 40°C (104°F) 40 cSt
Kinematic Viscosity at 100°C (212°F) 8.6 cSt
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 200 kg
Four Ball Wear 0.480 mm
Penetration 340Cone, worked 60 strokes; ASTM D217
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
USDA Yes
 
Descriptive Properties
AppearanceGolden

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ELM® SoyGrease™ EP Premium Biodegradable Extreme Pressure Grease, NLGI Grade 2
ELM® SoyGrease™ EP Plus Biodegradable Extreme Pressure Grease, NLGI Grade 3
ELM® SoyGrease™ EP Plus Biodegradable Extreme Pressure Grease, NLGI Grade 2
ELM® SoyGrease™ Biodegradable Grease for Semi-Truck Fifth Wheels
Cossa Polimeri ESTABIO EX 03120 B Biodegradable Plastic, Calcium Carbonate Filled

WELML002 / 146205

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.