MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Borealis Borcom™ BG055AI High Stiffness Polypropylene for Injection Molding Applications
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. BG055AI is a very easy flowing material with a good balance between impact strength and stiffness. The material provides high surface quality.

BG055AI is especially designed for air duct systems, climate control units, back-injection molding, and parts requiring high aesthetic surface finish.

Former trade name for this product was Xmod™

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183
Melt Flow  22 g/10 min
@Load 2.16 kg,
Temperature 230 °C
22 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 96 g/10 min
@Load 5.00 kg,
Temperature 230 °C
96 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 85.0 MPa12300 psiH 385/30; ISO 2039
Tensile Strength, Yield 35.0 MPa5080 psiAt 50 mm/min; ISO 527-2
Tensile Modulus 2.00 GPa290 ksiAt 1 mm/min; ISO 527-2
Flexural Modulus 1.85 GPa268 ksiAt 2 mm/min; ISO 178
Charpy Impact Unnotched 10.2 J/cm²48.5 ft-lb/in²ISO 179/1eU
 3.50 J/cm²
@Temperature -20.0 °C
16.7 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 0.150 J/cm²
@Temperature -20.0 °C
0.714 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C226 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-2
Vicat Softening Point 95.0 °C203 °FB (50N); ISO 306
 156 °C313 °FA (10N); ISO 306
Shrinkage 1.5 %
@Thickness 2.00 mm
1.5 %
@Thickness 0.0787 in
disk; Borealis Method
 
Optical PropertiesMetricEnglishComments
Gloss 75 %75 %20°; DIN 67530
 95 %95 %60°; DIN 67530
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 260 °C410 - 500 °FPolymer Mass Temp
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
 
Descriptive Properties
Emissions, ug C/g 30VDA 277
Fogging, mg1.1At 100°C/ 16 hours

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications
Borealis BE961MO Polypropylene for Injection Molding
Borealis BF970MO Polypropylene for Injection Molding
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled

PBOREA208 / 27515

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.