Elastocon® CLR45 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR45 is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® CLR45 can be overmolded onto polypropyleneInformation provided by Elastocon TPE Technologies, Inc. Elastocon® TPE Technologies has been acquired by Aurora Plastics. |