MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Hicor® 30 HT 183 OHD Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: One-side metallized, non-sealable, oriented high density polyethylene film, which has outstanding deadfold and directional tear characteristics. This film has been designed to be used in various applications, such as twistwrap and in laminations with other ExxonMobil Chemical OPP films, providing a new generation of laminates.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.18 mil
Coating Weight >= 17.2 lb/ream520
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.30430
Film Tensile Strength at Break, MD 5000 psi510
Film Tensile Strength at Break, TD 21700 psi510
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 1.7 %
@Temperature 135 °C
438
Shrinkage, TD 5.0 %
@Temperature 135 °C
438
 
Optical PropertiesOriginal ValueComments
Optical Density 1.8474
 
Descriptive Properties
Yield, in2/lb25100

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accutech Polyethylene HD0234G30UVL High Density Glass Reinforced UV Stabilized
NOVA Chemicals Sclair® 19G Homopolymer HDPE Film Resin
ExxonMobil Hicor® 30 HT 103 OHD Film
ExxonMobil Hicor® 30 HF 104 OHD Film
Aclo Accutech Polyethylene HD0234G40UVL High Density Glass Reinforced UV Stabilized

PEXB460 / 37765

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.