System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Techmer ES HiFill® PEI GF10 10% Glass Filled
Categories:
Polymer
;
Thermoplastic
;
Polyetherimide (PEI)
;
Polyetherimide (PEI), 10% Glass Fiber
Material Notes:
Availability: North America
Forms: Pellets
Filler/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight
Information provided by TP Composites, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.34
g/cc
ASTM D792
Water Absorption
0.22 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow
0.0050
in/in
@Thickness 3.17 mm
ASTM D955
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
17500
psi
ASTM D638
Flexural Strength
29500
psi
ASTM D790
Flexural Modulus
750000
psi
ASTM D790
Izod Impact, Notched
1.00
ft-lb/in
@Thickness 3.17 mm
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
410
°F
Unannealed; ASTM D648
Flammability, UL94
V-0
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Polyplastics Duranex® CRN7000 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%
Oxford Polymers 10GF 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI
Afton Plastics 2100 10% Glass Filled Polyetherimide
PTPC0492 / 136430
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.