Hostacom X M2 U34 82VTITANSCHWARZ medium melt flow, very high flexural modulus, mineral-filled PP homopolymer has high stiffness, low odor and high heat ageing stability. It is offered with an interior UV weathering stabilization package and in a specific OEM color match, for select interior trim applications. Applications: Interior Automotive ApplicationsInformation provided by LyondellBasell. |