MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Cosmic Plastics K61/6230 Long Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled

Material Notes: Description: Cosmic K61 / 6230 is a long glass fiber filled, general purpose diallyl iso-phthalate molding compound which is supplied in a flake form. It can be preformed and molds easily in standard compression or transfer equipment.

Features: It has excellent mechanical and electrical properties with a high dielectric strength and low dielectric constant. It has superior heat resistance and excellent machining qualities. K61 / 6230 has a shelf life of two years at room temperature with no reduction in performance.

Applications: The high strength of this material makes it ideal for switches, terminals, housings, structural parts and insulators.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.72 g/cc
Bulk Factor 6.0
Water Absorption 0.25 %
@Temperature 50.0 °C,
Time 173000 sec
Linear Mold Shrinkage 0.0010 - 0.0040 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 6000 - 10000 psi
Flexural Strength 13000 - 17000 psi
Compressive Strength 24000 - 30000 psi
Izod Impact, Notched 3.00 - 6.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cm
 3.00e+10 ohm-cm
@Temperature 70.0 °C,
Time 2.59e+6 sec
100% RH
Surface Resistance >= 1.00e+16 ohm
 5.00e+10 ohm
@Temperature 70.0 °C,
Time 2.59e+6 sec
100% RH
Dielectric Constant 3.8
@Frequency 1e+6 Hz
Dry
 3.9
@Frequency 1e+6 Hz
Wet
 4.0
@Frequency 1000 Hz
Dry
 4.1
@Frequency 1000 Hz
Wet
Dielectric Strength 400 V/milWet, step by step
 410 V/milDry, step by step
Dielectric Breakdown 60 VWet, step by step
 64 VDry, step by step
Dissipation Factor 0.0080
@Frequency 1000 Hz
Dry
 0.0090
@Frequency 1000 Hz
Wet
 0.012
@Frequency 1e+6 Hz
Dry
 0.013
@Frequency 1e+6 Hz
Wet
Arc Resistance 180 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 24.0 µm/m-°C
@Temperature -40.0 - 100 °C
Heat Distortion Temperature 260 °C
 
Processing PropertiesOriginal ValueComments
Mold Temperature 135 - 170 °C
 
Descriptive Properties
Dimensional Stability<0.01%
MIL-M-14GDI-30ASTM D5948-96
 GII-30ASTM D5948-96
Molding Pressure500-8000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite RX® 643 Phenolic Resole Compound
Cosmic Plastics D69/6130 Long Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound
PSM Industries Pacific Sintered Metals FCC-200-P High Carbon Copper Steel Powdered Metal (MPIF FC-0505-40)
PSM Industries Pacific Sintered Metals FCC-214-S High Carbon Copper Steel Powdered Metal (MPIF FC-0208-50)
Sumitomo Bakelite RX® 647 Phenolic Resole Compound

PCOSM013 / 190795

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.