Notes: Sarlink ME-2200N series is a general purpose thermoplastic elastomer series designed for a variety of automotive applications including exterior molded applications. Sarlink ME-2245N is a medium hardness, low density, UV stabilized grade suitable for injection molding. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Processability; Low Density; Medium Hardness; Low Specific Gravity; Light Stabilized; Low Flow; Lubricated; Sunlight Resistant; UV Resistant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Rubber Replacement RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |