MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® D139 m-LLDPE Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Low Density Polyethylene

Customer Benefits: Possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved processability (bubble stability, down-gauging, and melt fracture resistance). Has a puncture value of 18 kg as per ASTM D3763.

Data provided by Chevron Phillips Chemical Company, LP.

Formerly branded with the MarFlex® trade name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Melt Flow 0.90 g/10 minCondition 190/2.16; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 10.0 MPa2 in per min; ASTM D882
Film Tensile Strength at Yield, TD 10.0 MPa2 in per min; ASTM D882
Film Elongation at Break, MD 500 %2 in per min; ASTM D882
Film Elongation at Break, TD 600 %2 in per min; ASTM D882
Coefficient of Friction, Dynamic 0.70ASTM D1894
Coefficient of Friction, Static 1.0ASTM D1894
Elmendorf Tear Strength MD 210 gASTM D1922
Elmendorf Tear Strength TD 420 gASTM D1922
Dart Drop Test 800 gASTM D1709
Film Tensile Strength at Break, MD 34.0 MPa2 in per min; ASTM D882
Film Tensile Strength at Break, TD 28.0 MPa2 in per min; ASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 5.0 %ASTM D1003
 
Descriptive Properties
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® D143 m-LLDPE Linear Low Density Polyethylene
Chevron Phillips Marlex® D350 m-LLDPE Linear Low Density Polyethylene
Dow ELITE™ 5500G Enhanced Polyethylene Resin
Dow Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity

PCHEVP00 / 20340

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.