Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: High Gloss Uses: Automotive Interior Parts Automotive Specifications:CHRYSLER MS-DC 277 CPN2738 Color: Color As Noted On Drawing; CHRYSLER MS-DC 543 CPN4588 Color: 100% Color Match Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |