MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nishida Giken FULXUS® FX-TPV190 Thermo Plastic Olefin
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: In this olefin elastomer, we have finely dispersed EPDM in PP and we have done dynamic cross-linking with organic peroxide. EPDM is either partially or completely cross-linked.
  • Excellent weather resistance and chemical resistance
  • Because of low density, weight of the products can be reduced (0.88-0.89)
  • It is highly recyclable, and there is very little decline in properties even if it is reused
  • It has excellent heat resistance, and it has excellent extrusion and intrusion formability

Information provided by Nishida Giken

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 190 °C
20 g/10 min
@Load 11.0 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 9.20 MPa1330 psi
Elongation at Break 450 %450 %
100% Modulus 6.00 MPa870 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNISHG011 / 296202

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.