MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Proto3000 HP 3D High Reusability PA 11 3D Printing MultiJet Fusion Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11)

Material Notes: HP 3D High Reusability PA 11 is a thermoplastic nylon 3D printing powder engineered for the Multi Jet Fusion 3D printing process. It is used to produce functional parts with high strength and ductility for a wide variety of industries such as prostheses, insoles, sports goods, snap fits, living hinges, and more. The Nylon PA11 can assure high-quality standards of the 3D printed parts as well as performance in terms of durability, detailing, and accuracy. HP 3D High Reusability PA 11 is a polyamide (PA) material used in HP’s Multi Jet Fusion (MJF) 3D printing process. PA 11 is a thermoplastic Polymer Combination known for its toughness, chemical resistance, and high-temperature resistance. It is commonly used in the production of functional prototypes, end-use parts, and tooling. HP’s High Reusability PA 11 is specifically formulated to be highly durable and reusable, making it well-suited for applications that require parts with high strength and long-term performance. It is also easy to post-process and can be dyed or painted to achieve a wide range of colors.

Applications:

  • Medical - Prostheses, insoles
  • Production Parts - Strong and durable end-use parts such as living hinges or snap fits
  • Consumer goods - Sports goods, electronic devices
Characteristics
  • Biocompatibility—meets USP Class I-VI and US FDA guidance for Intact Skin Surface Devices
Uses
  • Prostheses
  • Insoles
  • Sport goods
  • Snap fits
  • Living hinges
Industries
  • Healthcare
  • Consumer goods
  • Industrial goods
  • Education
Certifications: USP Class I-VI and US FDA guidance for Intact Skin Surface Devices

Information provided by Proto3000

Key Words: MJF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.480 g/ccASTM D1895
Density 1.04 g/ccASTM D792
Particle Size 54.0 µmASTM D3451
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80.0XY, XZ, YX, YZ, ZX, ZY; ASTM D2240
Tensile Strength 52.0 MPamax load, ZX, ZY, 10 mm/min, specimens type V; ASTM D638
Elongation at Break 35.0 %ZX, ZY, 10 mm/min, specimens type V; ASTM D638
 50.0 %XY, XZ, YX, YZ, 10 mm/min, specimens type V; ASTM D638
Tensile Modulus 1800 MPaXY, XZ, YX, YZ, 10 mm/min, specimens type V; ASTM D638
 1800 MPaZX, ZY, 10 mm/min, specimens type V; ASTM D638
Flexural Strength 70.0 MPa
@Strain 5.0 %
XY, XZ, YX, YZ, ZX, ZY, Procedure B at a test rate of 13.55 mm/min; ASTM D790
Flexural Modulus 1800 MPaXY, XZ, YX, YZ, ZX, ZY, Procedure B at a test rate of 13.55 mm/min; ASTM D790
Izod Impact, Notched (ISO) 4.50 kJ/m²
@Thickness 3.20 mm
ZX, ZY; ASTM D256 Test Method A
 5.00 kJ/m²
@Thickness 3.20 mm
XY, XZ, YX, YZ; ASTM D256 Test Method A
 
Thermal PropertiesOriginal ValueComments
Melting Point 202 °CPowder; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 185 °CXY, XZ, YX, YZ, ZX, ZY; ASTM D648 Test Method A
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °CXY, XZ, YX, YZ, ZX, ZY; ASTM D648 Test Method A
 
Descriptive Properties
Refresh ratio for stable performance (%)30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPROTO802 / 322815

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.