MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Bromine, Br2
Categories: Fluid; Pure Element

Material Notes: CAS Number: 7726-95-6

Physical Form: Red Liquid

Key Words: Bromine, Br2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.1028 g/cc
Viscosity 0.996 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 159.808 g/mol
Vapor Pressure 173.339 torr
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 79.9041995
Atomic Number 35
X-ray Absorption Edge 0.91994 ÅK
 6.925 ÅLI
 7.7523 ÅLII
 7.9871 ÅLIII
Critical Pressure 102.048 atm
Critical Temperature 315 °C
Critical Density 1.258 g/cc
Critical Molar Volume 127 cm³/mol
Electronegativity 2.96Pauling
Ionic Radius 0.390 ÅCrystal Ionic Radius for Valence +7
 0.470 ÅCrystal Ionic Radius for Valence +5
 1.96 ÅCrystal Ionic Radius for Valence -1
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.15
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 65.83 J/g
Heat of Vaporization 187.5 J/gAt Boiling Point
 193.4 J/g
@Temperature 25.0 °C
Specific Heat Capacity 0.226 J/g-°C
 0.4737 J/g-°CLiquid
 0.229 J/g-°C
@Temperature 25.0 °C
Vapor
Thermal Conductivity 0.123 W/m-K
@Temperature 20.0 °C
Melting Point -7.20 °C
Boiling Point 58.8 °C
Heat of Formation 0.000 kJ/molLiquid
 30.9 kJ/molGas
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.659
@Temperature 15.0 °C,
Wavelength 589 nm
 
Component Elements PropertiesOriginal ValueComments
Bromine, Br 100 %
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter15.8441
Antoine's Vapor Pressure B Parameter2582.32
Antoine's Vapor Pressure C Parameter-51.56
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
AppearanceRed Liquid
CAS Number7726-95-6
Critical Compressibility (Zc)0.27
Dipole moment (p/C.m)6.671E-29
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A387.82
Dynamic Viscosity Parameter B292.79
Molar Heat Capacity (298K)36.521 J/mol-K
Molar Heat Capacity of Vapor a Parameter33.836
Molar Heat Capacity of Vapor b Parameter0.0112
Molar Heat Capacity of Vapor c Parameter-1.191E-05
Molar Heat Capacity of Vapor d Parameter4.531E-09
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
SolubilitySoluble in H2O

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fluorine, F2
Argon, Ar
Chlorine, Cl2
Helium, He
Neon, Ne

AMEBr / 15

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.