MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EOS MaragingSteel MS1 DMSL on EOS M 400-4
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Maraging Steel

Material Notes: EOS MaragingSteel MS1 has a chemical composition following US classification 18% Ni Maraging 300, European 1.2709 and German X3NiCoMoTi 18-9-5. This kind of steel is characterized by having very good mechanical properties, and being easily heat-treatable using a simple thermal age-hardening process to obtain excellent hardness and strength. Parts built from EOS MaragingSteel MS1 are easily machinable after the building process and can be easily post-hardened to more than 50 HRC by age-hardening at 490 °C (914 °F) for 6 hours. In both as-built and age-hardened states the parts can be machined, spark-eroded, weld-ed, micro shot-peened, polished and coated if required.

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 - 8.10 g/cc0.289 - 0.293 lb/in³ISO 3369
Particle Size <= 63 µm<= 63 µm<0.5 wt% above 63µm; ASTM B214
Thickness 40.0 microns1.57 milLayer Thickness
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 50 - 75
@Treatment Temp. 490 °C,
Time 21600 sec
50 - 75
@Treatment Temp. 914 °F,
Time 6.00 hour
heat treated; EN ISO 6508-1
Tensile Strength, Ultimate 1200 MPa174000 psiAs built, Horizontal; ISO 6892-1 B10
 1200 MPa174000 psiAs built, Vertical; ISO 6892-1 B10
 2060 MPa
@Treatment Temp. 490 °C,
Time 21600 sec
299000 psi
@Treatment Temp. 914 °F,
Time 6.00 hour
Heat treated horizontal; ISO 6892-1 B10
 2080 MPa
@Treatment Temp. 490 °C,
Time 21600 sec
302000 psi
@Treatment Temp. 914 °F,
Time 6.00 hour
Heat treated vertical; ISO 6892-1 B10
Tensile Strength, Yield 1020 MPa148000 psiAs built, Horizontal; ISO 6892-1 B10
 1050 MPa152000 psiAs built, Vertical; ISO 6892-1 B10
 1990 MPa
@Treatment Temp. 490 °C,
Time 21600 sec
289000 psi
@Treatment Temp. 914 °F,
Time 6.00 hour
Heat treated horizontal; ISO 6892-1 B10
 2010 MPa
@Treatment Temp. 490 °C,
Time 21600 sec
292000 psi
@Treatment Temp. 914 °F,
Time 6.00 hour
Heat treated vertical; ISO 6892-1 B10
Elongation at Break 11 %11 %As built, Vertical; ISO 6892-1 B10
 13 %13 %As built, Horizontal; ISO 6892-1 B10
 3.0 %
@Treatment Temp. 490 °C,
Time 21600 sec
3.0 %
@Treatment Temp. 914 °F,
Time 6.00 hour
Heat treated vertical; ISO 6892-1 B10
 4.0 %
@Treatment Temp. 490 °C,
Time 21600 sec
4.0 %
@Treatment Temp. 914 °F,
Time 6.00 hour
Heat treated horizontal; ISO 6892-1 B10
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.050 - 0.15 %0.050 - 0.15 %
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr <= 0.50 %<= 0.50 %
Cobalt, Co 8.5 - 9.5 %8.5 - 9.5 %
Copper, Cu <= 0.50 %<= 0.50 %
Iron, Fe 64.1 - 69.35 %64.1 - 69.35 %Balance
Manganese, Mn <= 0.10 %<= 0.10 %
Molybdenum, Mo 4.5 - 5.2 %4.5 - 5.2 %
Nickel, Ni 17 - 19 %17 - 19 %
Phosphorus, P <= 0.010 %<= 0.010 %
Silicon, Si <= 0.10 %<= 0.10 %
Sulfur, S <= 0.010 %<= 0.010 %
Titanium, Ti 0.60 - 0.80 %0.60 - 0.80 %
 
Descriptive Properties
Surface roughness20-50 µmRz, after shot peening
 4-6.5 µmRa, after shot peening
Volume rateUp to 4 x 4.2 mm³/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS970 / 280630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.