MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® R513H BK02 Nylon 66, 13% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Vydyne R513H BK02 is a general purpose, 13% glass-filled, heat-stabilized PA66 based resin designed for injection molding applications. R513H BK02 offers improved flow with a black surface finish and maintains the excellent resistance typical of PA66 in chemicals, machine and motor oils, solvents, and gasoline.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccDAM; ISO 1183
Water Absorption 1.0 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 2.2 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPa50% RH; ISO 527-2
 115 MPaDAM; ISO 527-2
Elongation at Break 3.0 %DAM; ISO 527-2
 13 %50% RH; ISO 527-2
Tensile Modulus 3900 MPa50% RH; ISO 527-2
 6200 MPaDAM; ISO 527-2
Flexural Strength 106 MPa50% RH; ISO 178
 165 MPaDAM; ISO 178
Flexural Modulus 3150 MPa50% RH; ISO 178
 5200 MPaDAM; ISO 178
Poissons Ratio 0.40ISO 527-2
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 5.10 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 5.40 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 8.50 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 31.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 37.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 38.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 42.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 5.30 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 6.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 7.50 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
Dielectric Strength 20.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
PLC 6; ASTM D 495
Comparative Tracking Index 250 - 399 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 secPLC 4; UL 746
 7.0 - 15 secPLC 4; UL 746
 15 - 30 secPLC 3; UL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minPLC 1; UL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 113 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 240 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 140 °C
@Thickness 0.750 mm
UL 746
 140 °C
@Thickness 1.50 mm
UL 746
 140 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 120 °C
@Thickness 0.750 mm
UL 746
 120 °C
@Thickness 1.50 mm
UL 746
 120 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 125 °C
@Thickness 0.750 mm
UL 746
 140 °C
@Thickness 1.50 mm
UL 746
 140 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 0.750 mm
 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
Oxygen Index 25 %DAM; EN ISO 4589-2
 25 %Railway Application; DAM; EN ISO 4589-2
Glow Wire Ignition Temperature 700 °C
@Thickness 0.400 mm
IEC 60695-2-13
 700 °C
@Thickness 0.750 mm
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
IEC 60695-2-13
Glow Wire Flammability Index 675 °C
@Thickness 0.400 mm
IEC 60695-2-12
 675 °C
@Thickness 0.750 mm
IEC 60695-2-12
 675 °C
@Thickness 1.50 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection
Middle Barrel Temperature 280 - 310 °CInjection
Front Barrel Temperature 280 - 310 °CInjection
Nozzle Temperature 280 - 310 °CInjection
Melt Temperature 285 - 305 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066 PA012G15
 ASTM, D6779 PA012G15
 SAE, J1639 PA1112
AppearanceBlack
Automotive Material SpecificationDelphi M4147V
FeaturesChemical Resistant
 Gasoline Resistant
 Good Mold Release
 Grease Resistant
 High Flow
 High Rigidity
 High Strength
 Lubricated
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 70G13HS1L BK031 PA66-GF13
Ascend Performance Materials Vydyne® R413H BK07 Impact Modified Nylon 66, 13% Glass Filled
Thermal Ceramics Superwool 607 Pyro-Fold and Pyro-Stack Modules
Thermal Ceramics Superwool 607 Max Pyro-Fold and Pyro-Stack Modules
Zircar Zirconia ZYC Zirconia Cylinders Insulation

PASCE9778 / 220881

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.