MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes:
  • 40% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.
  • Drop-in replacement for other commercially available 40% glass sphere filled PA 12 laser sintering powders.
  • More recyclable, produces a better part surface finish, and the dry powder flow has been optimized

Information provided by Advanced Laser Materials (ALM).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.630 g/ccASTM D1895
Density 1.22 g/ccSintered; ASTM D792
Particle Size 57 µmD50
 35 - 100 µmD10-D90
Melt Flow 50 g/10 min
@Load 5.00 kg,
Temperature 235 °C
3 min; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 51.0 MPaXY; ASTM D638
Elongation at Break 9.0 %XY; ASTM D638
Tensile Modulus 3200 MPaXY; ASTM D638
Flexural Modulus 2900 MPaXY; ASTM D790
Izod Impact, Notched 42.0 J/mASTM D256
Izod Impact, Unnotched 213 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cm50% RH, 500V; ASTM D257
Surface Resistance 2.30e+14 ohm50% RH, 500V; ASTM D257
Dielectric Constant 3.7ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 186 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 175 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Celanese VECTRA® T130 30% Glass Filled Liquid Crystal Polymer (LCP)
Mitsubishi Chemical Advanced Materials Ertalyte™ PET Polyester-semi-crystalline thermoplastic, extruded
Hippe PA 12 Nylon 12

PALP84 / 177145

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.