MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petropol Thanelene® B3 95A HL UV CRLA010 TP312 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Product Description: Hardness 95 shore A, Thermoplastic Polyurethane

Resin ID (ISO 1043): TPU
Additive: UV resistant, Superior Release
Processing: Injection Molding, Extrusion
Color: Transparent

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.211 g/cc0.04375 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ISO 868
Hardness, Shore D 4040ISO 868
Tensile Strength, Ultimate 55.0 MPa7980 psiISO 527
Tensile Stress  8.00 MPa
@Strain 100 %
1160 psi
@Strain 100 %
ISO 527
 24.0 MPa
@Strain 300 %
3480 psi
@Strain 300 %
ISO 527
Elongation at Break 430 %430 %ISO 527
Flexural Modulus  0.0300 GPa
@Temperature 70.0 °C
4.35 ksi
@Temperature 158 °F
Torsional Storage; ISO 6721-2
 0.0540 GPa
@Temperature 23.0 °C
7.83 ksi
@Temperature 73.4 °F
Torsional Storage; ISO 6721-2
 0.848 GPa
@Temperature -20.0 °C
123 ksi
@Temperature -4.00 °F
Torsional Storage; ISO 6721-2
Resilience 2929[%], Impact Resilience; ISO 4662
Tear Strength 95.0 kN/m542 pliPropagation; ISO 34-1
Abrasion 2222[mm3]; ISO 4649
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 210 °C356 - 410 °FExtrusion
 215 - 235 °C419 - 455 °FInjection Molding
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 hour3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL406 / 313314

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.