MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borcoat™ MA115E Syntactic Polypropylene for Steel Pipe Coating  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Borcoat™ MA115E is a highly filled polypropylene compound and is self colored. Applications: Borcoat™ MA115E is recommended as heavy weight coating for special applications used in steel pipe coating.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³ISO 1183
Filler Content 70 %70 %
Melt Flow 2.8 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.8 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.0 MPa2610 psi50mm/min; ISO 527-2
Elongation at Break 50 %50 %50mm/min; ISO 527-2
Elongation at Yield 1.8 %1.8 %ISO 527-2
Tensile Modulus 3.50 GPa508 ksi1mm/min; ISO 527-2
Charpy Impact, Notched  0.120 J/cm²
@Temperature -20.0 °C
0.571 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 0.190 J/cm²
@Temperature 23.0 °C
0.904 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FISO 75-2
Vicat Softening Point 105 °C221 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 200 - 220 °C392 - 428 °Fcylinder
Die Temperature 210 - 220 °C410 - 428 °F
Melt Temperature 210 - 230 °C410 - 446 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis KSR4525 Polypropylene Reactor Elastomer Modified
Borealis BA11CF Polypropylene Copolymer
A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion
Borealis BorPURE™ RE450MO Polypropylene Random Copolymer
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer

PBOREA366 / 108626

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.