MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wingate Alloys Winco-Tuf 40 High Strength Wear Plate
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Quenched and tempered for extreme abrasion and moderate impact.

Winco-Tuf 40 has excellent toughness at high hardness and in heavy sections. For severe abrasions.

    Advantages:
  • Maximum resistance to abrasion and impact.
  • Withstands the brittleness which develops at subnormal temperatures.
  • Increased toughness and fatigue resistance compared to low carbon and 1045 plate.
  • Retains high strength and wearability at high temperatures.
  • High impact and wear properties retained at weld joints.

Information from Wingate Alloys Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 375 - 440
Hardness, Rockwell C 40 - 46
Tensile Strength 200000 psi
Tensile Strength, Yield 160000 psi
Elongation at Break 14.4 %2[in]
Reduction of Area 55 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.17 - 0.25 %
Chromium, Cr 0.45 - 0.60 %
Copper, Cu 0.15 - 0.30 %
Iron, Fe 95.21 - 96.33 %
Manganese, Mn 1.5 %
Molybdenum, Mo 0.20 - 0.60 %
Nickel, Ni 0.70 - 1.0 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.50 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SSAB Tunnplat Domex® Wear Steel Sheet
The NanoSteel® Company SHS 9700 Steel Alloy, Wear Plate
AISI 1045 Steel, cold drawn, low temperature, stress relieved round (16 - 22 mm)
AISI 1045 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
AISI 1045 Steel, cold drawn, high temperature stress relieved, 50-75 mm (2-3 in) round

NWINGA02 / 122066

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.