System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Polyram RamLloy PBB520 PC/ABS alloy, Flame Retardant
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
;
Polycarbonate (PC)
Material Notes:
Flame retardant PC/ABS alloy for injection molding applications
Information provided by Polyram Ram On Ind.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.13
g/cc
0.0408
lb/in³
DIN 53479
Linear Mold Shrinkage
0.0050
-
0.0080
cm/cm
0.0050
-
0.0080
in/in
Melt Flow
25
g/10 min
@Load 5.00 kg,
Temperature 240 °C
25
g/10 min
@Load 11.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
50.0
MPa
7250
psi
ASTM-D638
Elongation at Break
25 %
25 %
ASTM-D638
Tensile Modulus
2.20
GPa
319
ksi
ASTM-D790
Izod Impact, Notched
3.50
J/cm
@Temperature 23.0 °C
6.56
ft-lb/in
@Temperature 73.4 °F
ASTM-D256
Electrical Properties
Metric
English
Comments
Surface Resistance
1.00e+14
ohm
1.00e+14
ohm
DIN 53482
Dielectric Strength
24.0
kV/mm
610
kV/in
VDE 0303/4
Thermal Properties
Metric
English
Comments
Glow Wire Test
960
°C
1760
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Extruded
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Chlorinated PVC (CPVC)
Overview of materials for Cellulose Acetate, Molded
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
PPOLYRA351 / 57613
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.