MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Michelman® Michem ® Flex HS268 Water-based Heat Seal Coating
Categories: Fluid; Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Water-based heat seal coating for flexible packaging. Michem® Flex HS 268 can be applied via rod, gravure, and spray. Usage: Used for heat sealing applications offering low temperature seal initiation and stronger bonds to paper, metal (foil or metalized surface), various primed films such as matte, pearlized cavitated BOPP or BOPET films. It should be used with the addition of a wax emulsion to control the coefficient of friction (typically 2 to 4% by weight) e.g. Michem® Lube 160 RPH.

Applications (properties imparted): Heat Seal Coatings (Substrate - film, Substrate - paper, metal).

Handling: Ensure adequate ventilation. Handle in accordance with good industrial hygiene and safety practice.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 - 0.970 g/cc0.950 - 0.970 g/cc
Solids Content 36 - 39 %36 - 39 %Non-Volatiles
pH 9.4 - 10.59.4 - 10.5
Brookfield Viscosity 100 - 350 cP100 - 350 cPSpindle #3. 50 RPM.
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceWhite to off-white liquid
EZ Cup Viscosity (sec)33 - 35Cup #3
Freeze/Thaw StabilityNone: protect from freezing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHE9822 / 287417

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.