MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC LNP™ LUBRICOMP™ Compound OL004 Polyphenylene Sulfide, Linear (PPS, Linear)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LNP LUBRICOMP OL004 compound is based on Polyphenylene Sulfide (PPS) - linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ASTM D792
 1.45 g/cc0.0524 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.010 - 0.030 cm/cm0.010 - 0.030 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm0.010 - 0.030 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psi5 mm/min; ASTM D638
 58.0 MPa8410 psi5 mm/min; ISO 527
Tensile Strength, Yield 53.0 MPa7690 psi5 mm/min; ASTM D638
 58.0 MPa8410 psi5 mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5 mm/min; ASTM D638
 4.0 %4.0 %5 mm/min; ISO 527
Elongation at Yield 3.0 %3.0 %5 mm/min; ASTM D638
 4.6 %4.6 %5 mm/min; ISO 527
Tensile Modulus 3.00 GPa435 ksi50 mm/min; ASTM D638
 3.10 GPa450 ksi1 mm/min; ISO 527
Flexural Strength 96.0 MPa13900 psi1.3 mm/min, 50 mm span; ASTM D790
 97.0 MPa14100 psi2 mm/min; ISO 178
Flexural Modulus 2.84 GPa412 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.95 GPa428 ksi2 mm/min; ISO 178
Izod Impact Notched 32.0 J23.6 ft-lbASTM D256
Izod Impact, Unnotched 3.48 J/cm6.52 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 2.00 J1.48 ft-lbpeak; ASTM D3763
Coefficient of Friction, Dynamic 0.210.21ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.0800.080ASTM D3702 Modified: Manual
K (wear) Factor 169 x 10-8 mm³/N-M84.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 52.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 53.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
29.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 179 °C354 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 129 °C
@Thickness 3.20 mm
264 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 102 °C216 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 99.0 °C
@Thickness 3.20 mm
210 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 130 °C266 °FUL 746B
UL RTI, Mechanical without Impact 130 °C266 °FUL 746B
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 320 - 330 °C608 - 626 °F
Zone 3 330 - 345 °C626 - 653 °F
Melt Temperature 315 - 320 °C599 - 608 °FInjection Molding
Mold Temperature 140 - 165 °C284 - 329 °F
Drying Temperature 120 - 150 °C248 - 302 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80930 / 288877

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.