MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carlisle 201HL Carbon-Carbon Composite
Categories: Carbon

Material Notes: Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air to 750F (400C) and can be used to 3600F (2000C) when protected by an inert environment or vacuum. Key attributes include thermal shock resistance, fracture toughness, corrosion resistance, electrical conductivity, temperature stability, with a very low coefficient of thermal expansion. Machines quite well with intricate features possible for complex shapes. Common applications include hot glass handling tooling, powdered metal sintering trays, atmosphere and vacuum furnace racks and hardware, spark plasma sintering dies, high temperature nuts, bolts, fasteners, racing brakes and clutches, sputtering targets, and components used in energy production.

Information provided by Carlisle Brake & Friction.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 1.65 g/cc
Porosity 13 %Total
Ash 0.0021 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 10.0 ksiin plane
Modulus of Elasticity 5200 ksi
Flexural Strength 12.0 ksiperpendicular
 15.0 ksiin plane
Flexural Modulus 4000 ksi
Compressive Strength 8.00 ksiperpendicular
 12.0 ksiin plane
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00240 ohm-cm
@Temperature 17.0 °C
in plane
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.00 µm/m-°C
@Temperature 23.0 - 1500 °C
Secant Value
CTE, linear, Transverse to Flow 7.00 µm/m-°C
@Temperature 23.0 - 1500 °C
Secant Value
Specific Heat Capacity 0.850 J/g-°C
@Temperature 50.0 °C
 1.30 J/g-°C
@Temperature 250 °C
Thermal Conductivity 20.0 W/m-Kperpendicular
 50.0 W/m-Kin plane
Maximum Service Temperature, Air 400 °C
Maximum Service Temperature, Inert 2000 °C
 
Descriptive Properties
Hardness, Rockwell 15X65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carlisle 201HD Carbon-Carbon Composite
Carlisle 201LD Carbon-Carbon Composite
Goodfellow Carbon-Carbon Composite
Carlisle 201LL Carbon-Carbon Composite
Graphite, Carbon, C

CCARLI991 / 171751

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.