MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teijin Multilon T-3011 Standard PC/ABS Polymer Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: General grade of PC/ABS polymer alloy, having improved impact strength and heat resistance compared with a heat resistant ABS and flame retardant m-PPE and also having higher fluidity compared with a heat resistant ABS.

Applications:

  • Mechanical components. Electric and electronic components, Safety and industrial equipment components.
  • Information provided by Teijin Chemicals Ltd.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.14 g/ccISO 1183
    Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
    @Thickness 4.00 mm
    Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
    @Thickness 4.00 mm
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength at Break 55.0 MPa50mm/min; ISO 527
    Tensile Strength, Yield 60.0 MPa50mm/min; ISO 527
    Elongation at Break 110 %50mm/min; ISO 527
    Elongation at Yield 3.0 %50mm/min; ISO 527
    Tensile Modulus 2.45 GPa1mm/min; ISO 527
    Flexural Strength 90.0 MPa2mm/min; ISO 178
    Flexural Modulus 2.50 GPa2mm/min; ISO 178
    Charpy Impact Unnotched NBISO 179
    Charpy Impact, Notched 8.00 J/cm²ISO 179
     
    Electrical PropertiesOriginal ValueComments
    Surface Resistance 1.00e+16 ohmIEC 60093
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 80.0 µm/m-°C
    @Temperature 20.0 °C
    ISO 11359
    CTE, linear, Transverse to Flow 80.0 µm/m-°C
    @Temperature 20.0 °C
    ISO 11359
    Deflection Temperature at 0.46 MPa (66 psi) 123 °CISO 75
    Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75
    Vicat Softening Point 121 °C50°C/hr, 50N; ISO 306
    Flammability, UL94 HB
    @Thickness 0.800 mm

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Teijin Multilon DN-1520B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
    Covestro Bayblend® T88-4N Polycarbonate + ABS, 20% Glass Filled
    Teijin Multilon T-3713 Standard PC/ABS Polymer Alloy
    Teijin Multilon T-2711 Standard, Automobile Part Series PC/ABS Polymer Alloy
    Teijin Multilon DN-3510F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy

    PTEIJ42 / 69731

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.