MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Latrobe LSS™ 420 Supreme Plastic Mold Steel (AISI 420)
Categories: Metal; Ferrous Metal; Stainless Steel; Tool Steel; Mold Steel

Material Notes: TLS 420 Supreme is a specially-refined, mold-quality stainless steel that is engineered to provide supreme polishability, good corrosion resistance, and good wear resistance. TLS 420 supreme is manufactured using special melting and remelting techniques. These special melting practices along with proprietary forging practices result in the highest levels of microcleanliness and a homogeneous microstructure. TLS 420 Supreme is the material of choice for the manufacture of plastic molding tools that require the highest lens-quality polished finishes. Typical applications include molds for compact disks (CDs), medical laboratory equipment, optical lenses, and other components, which require critical surface finishes.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.75 g/cc7.75 g/cc
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5252Air Cooled from 982°C, 30 minutes
 55.555.5Air Cooled from 1010°C, 30 minutes
 56.556.5Air Cooled from 1038°C, 30 minutes
Modulus of Elasticity 200 GPa29000 ksi
Machinability 55 - 60 %55 - 60 %1% Carbon Steel
Izod Impact Unnotched 13.6 J10.0 ft-lbAir Cooled from 1010°C; 393°C Temper Temperature
 20.3 J15.0 ft-lbAir Cooled from 1010°C; 593°C Temper Temperature
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.2 µm/m-°C
@Temperature 20.0 - 100 °C
5.67 µin/in-°F
@Temperature 68.0 - 212 °F
 11.7 µm/m-°C
@Temperature 20.0 - 538 °C
6.50 µin/in-°F
@Temperature 68.0 - 1000 °F
Thermal Conductivity  22.84 W/m-K
@Temperature 20.0 °C
158.5 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 23.93 W/m-K
@Temperature 199 °C
166.1 BTU-in/hr-ft²-°F
@Temperature 390 °F
 24.95 W/m-K
@Temperature 399 °C
173.2 BTU-in/hr-ft²-°F
@Temperature 750 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 802 °C1480 °FCritical Temperaure Ac1
 863 °C1590 °FCritical Temperaure Ac3
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 13.6 %13.6 %
Iron, Fe 84.87 %84.87 %
Manganese, Mn 0.45 %0.45 %
Other 0.38 %0.38 %
Silicon, Si 0.40 %0.40 %
Vanadium, V 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type P20 Mold Steel (UNS T51620)
Assab Steels MOLDMAX LH/MM Copper Alloy for Plastic Molds
ATI Allvac® VascoMax® C-250 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
International Mold Steel NAK55 Precipitation Hardened Mold Steel
International Mold Steel Premium H13 Hot Work Die and Mold Steel

NTIMK131 / 19478

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.