Westlake EB169 is a low-density polyethylene with high stiffness designed for beverage shrink overwrap and towel/tissue packaging. It has good toughness and blends well with LLDPE resins.Application/Uses- Beverage overwrap shrink film
- Light and medium duty produce bags
- Clarity packaging
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical |
Good toughness and blends well with LLDPE resins |